Optical constants of KTaO3 (Potassium tantalate)
Fujii and Sakudo 1976: n 0.4–1.06 µm

Wavelength: µm
 (0.4–1.06)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{3.591λ^2}{λ^2-0.193^2}$$

Notes

300 K (27 °C)

References

Y. Fujii and T. Sakudo. Dielectric and optical properties of KTaO3. J. Phys. Soc. Jpn. 41, 888-893 (1976).

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Potassium tantalate

Potassium tantalate (KTaO3) is a perovskite-structured crystal that has garnered interest in the field of optics and electronics. With its good mechanical and optical properties, KTaO3 serves as a substrate for epitaxial growth of various complex oxides. Additionally, it is used in a variety of applications, including electro-optic modulators, pyroelectric detectors, and nonlinear optics. The material is transparent in the visible and infrared regions, making it valuable for a range of light-based technologies. It is generally non-toxic but should be handled with the usual precautions for chemicals and materials.