Optical constants of KF (Potassium fluoride)
Li 1976: n 0.15–22 µm
Complex refractive index (n+ik)
Derived optical constants
Dispersion formula
$$n^2-1=0.55083+\frac{0.29162λ^2}{λ^2-0.126^2}+\frac{3.60001λ^2}{λ^2-51.55^2}$$Notes
297 K (24 °C).
References
H. H. Li.
Refractive index of alkali halides and its wavelength and temperature derivatives.
J. Phys. Chem. Ref. Data 5, 329-528 (1976) and references therein.
- Sellmeier formula is derived by critical analysis of experimental data from several sources.
Data
Additional information
About Potassium fluoride
Potassium fluoride (KF) is a crystalline material with particular usefulness in optical applications. It exhibits good transmission properties in the ultraviolet to the mid-infrared spectral regions. Unlike potassium chloride or bromide, it offers better moisture resistance, making it more versatile for use in environmental conditions that include some humidity. Frequently, KF is employed in windows and lenses for specialized optical systems, particularly those operating in the ultraviolet range. However, users should still exercise caution while handling it, as potassium fluoride can be corrosive. Overall, its combination of optical and chemical properties makes it a valuable material in various optical applications.
Other names and variations
- KF
- Potassium(I) fluoride