Optical constants of K108 (LZOS)
Bassarab et al. 2023: n,k 0.185–150000 µm
Wavelength:
µm
(0.18503–150000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
References