Optical constants of In2O3-SnO2 (Indium tin oxide, ITO)
Moerland and Hoogenboom 2016: n,k 0.4–1.0 µm

Wavelength: µm
 (0.401047791–0.999961060)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

film_thickness: 1.7E-8
substrate: glass

Notes

17 nm ITO film on D263M glass substrate. Purchased from Optics Balzers. Surface roughness (1 sigma) = 0.4 nm. Variable angle spectroscopic ellipsometry data + normal-incidence transmittance data fitted over the 400 to 900 nm range.

References

R. J. Moerland and J. P. Hoogenboom. Subnanometer-accuracy optical distance ruler based on fluorescence quenching by transparent conductors. Optica 3, 112-117 (2016) (See Supplementary materials. Numerical data kindly provided by Robert Moerland)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Indium tin oxide

Other names and variations

  • ITO
  • In2O3-SnO2
  • Tin-doped indium oxide

Links