Optical constants of In2O3-SnO2 (Indium tin oxide, ITO)
Minenkov et al. 2024: on glass; n,k 0.191–1.69 µm

Wavelength: µm
 (0.19146–1.68869)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

film_thickness: 1.1E-7
substrate: glass

Notes

110 nm thick ITO layer on glass type XY15S purchased from Xinyan Technology LTD.

References

A. Minenkov, S. Hollweger, J. Duchoslav, O. Erdene-Ochir, M. Weise, E. Ermilova, A. Hertwig, M. Schiek. Monitoring the electrochemical failure of indium tin oxide electrodes via operando ellipsometry. ACS Appl Mater Interfaces 16, 9517-9531 (2024) (Numerical data kindly provided by Manuela Schiek)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Indium tin oxide

Other names and variations

  • ITO
  • In2O3-SnO2
  • Tin-doped indium oxide

Links