Optical constants of In2O3-SnO2 (Indium tin oxide, ITO)
König et al. 2014: n,k 0.25–1.0 µm
Wavelength:
µm
(0.25157–1.00000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions
film_thickness: 7.2E-8 substrate: glass
Comments
72 nm ITO film on BK7 glass substrate. Purchased from Delta Technology (CG-60IN-CUV), 15–25 ohms. ITO includes a separate roughness layer (see \with EMA")"
References
T. A. F. König, P. A. Ledin, J. Kerszulis, M. A. Mahmoud, M. A. El-Sayed, J. R. Reynolds, V. V. Tsukruk. Electrically tunable plasmonic behavior of nanocube-polymer nanomaterials induced by a redox-active electrochromic polymer. ACS Nano 8, 6182-6192 (2014) (Numerical data kindly provided by Tobias König)
Data
Additional information
About Indium tin oxide
Other names and variations
- ITO
- In2O3-SnO2
- Tin-doped indium oxide