RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of In (Indium)
Mathewson and Myers 1971: n,k 0.344–1.77 µm; 140 K

Wavelength: µm
 (0.34440–1.77120)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

temperature: 140

Notes

140 K (-133.15 °C)

References

A. G. Mathewson and H. P. Myers. Absolute values of the optical constants of some pure metals. Phys. Scr. 4, 291-292 (1971)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Indium

Indium (In) is a soft, malleable metal that is primarily used in the electronics industry for making semiconductors, transistors, and a variety of other components. In the realm of optics, indium is often employed in the fabrication of photodetectors and infrared sensors due to its unique electronic properties. Indium-tin oxide (ITO) is a transparent conductive oxide that serves as a popular material for making touch screens, LED displays, and solar cells. Indium is also frequently used to create low-melting alloys for a variety of other technological applications. Despite its widespread use, indium is relatively rare and expensive. Precautions should be taken when handling indium compounds due to potential toxicity.

Other names and variations

  • In

Links