Optical constants of ISUZU - Optical glass filters
ISK370
Wavelength:
µm
(0.200–2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Notes
Heat absorbing filter (ISK series). Glass type: P2O5-Al2O3.
References
Data kindly provided by Koichiro Ikeda, ISUZU GLASS LTD. Nov 2024.
See also Isuzu Glass Products
Data
Additional information
Properties of ISK370
nd: 1.509
Vd: 84.8
density:
-
value: 2580
thermal_expansion:
-
temperature_range: 373 573
value: 5.8E-6
transformation_temperature:
-
value: 857
durability: 1
hardness:
-
type: Knoop
value: 4730000000
About Isuzu Glass Ltd.
Established in 1905 and headquartered in Osaka, Japan, Isuzu Glass Ltd. specializes in manufacturing molded glass lenses and optical filters. Their product range includes colored optical glasses and lenses utilized in projectors, lasers, medical devices, sensors, semiconductors, and energy equipment.