RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of ISUZU - Optical glass filters
ISK153

Wavelength: µm
 (0.200–2.000)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Heat absorbing filter (ISK series). Glass type: P2O5-Al2O3.

References

Data kindly provided by Koichiro Ikeda, ISUZU GLASS LTD. Nov 2024.
See also Isuzu Glass Products

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

Properties of ISK153

nd: 1.522
Vd: 65.2
density:
  - 
    value: 2610
thermal_expansion:
  - 
    temperature_range: 373 573
    value: 5.9E-6
transformation_temperature:
  - 
    value: 871
durability: 1
hardness:
  - 
    type: Knoop
    value: 4720000000

About Isuzu Glass Ltd.

Established in 1905 and headquartered in Osaka, Japan, Isuzu Glass Ltd. specializes in manufacturing molded glass lenses and optical filters. Their product range includes colored optical glasses and lenses utilized in projectors, lasers, medical devices, sensors, semiconductors, and energy equipment.

Links