Optical constants of ISUZU - Optical glass filters
ISK150
Wavelength:
µm
(0.200–2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Notes
Heat absorbing filter (ISK series). Glass type: P2O5-Al2O3.
References
Data kindly provided by Koichiro Ikeda, ISUZU GLASS LTD. Nov 2024.
See also Isuzu Glass Products
Data
Additional information
Properties of ISK150
nd: 1.516
Vd: "86.0"
density:
-
value: 2600
thermal_expansion:
-
temperature_range: 373 573
value: 6.0E-6
transformation_temperature:
-
value: 867
durability: 1
hardness:
-
type: Knoop
value: 4870000000
About Isuzu Glass Ltd.
Established in 1905 and headquartered in Osaka, Japan, Isuzu Glass Ltd. specializes in manufacturing molded glass lenses and optical filters. Their product range includes colored optical glasses and lenses utilized in projectors, lasers, medical devices, sensors, semiconductors, and energy equipment.