Optical constants of ISUZU - Optical glass filters
IHU310
Wavelength:
µm
(0.200–2.000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Notes
UV transmitting filter (IHU series). Glass type: SiO2-CaO-Na2O.
References
Data kindly provided by Koichiro Ikeda, ISUZU GLASS LTD. Nov 2024.
See also Isuzu Glass Products
Data
Additional information
Properties of IHU310
nd: 1.523
Vd: 58.2
density:
-
value: 2550
thermal_expansion:
-
temperature_range: 373 573
value: 9.4-06
transformation_temperature:
-
value: 806
durability: 3
hardness:
-
type: Knoop
value: 5320000000
About Isuzu Glass Ltd.
Established in 1905 and headquartered in Osaka, Japan, Isuzu Glass Ltd. specializes in manufacturing molded glass lenses and optical filters. Their product range includes colored optical glasses and lenses utilized in projectors, lasers, medical devices, sensors, semiconductors, and energy equipment.