Optical constants of ISUZU - Optical glass filters
IHU250H

Wavelength: µm
 (0.200–2.000)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

UV transmitting filter (IHU series). Glass type: SiO2-B2O3.

References

Data kindly provided by Koichiro Ikeda, ISUZU GLASS LTD. Nov 2024.
See also Isuzu Glass Products

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

Properties of IHU250H

nd: 1.504
Vd: 61.2
density:
  - 
    value: 2290
thermal_expansion:
  - 
    temperature_range: 373 573
    value: 7.9-06
transformation_temperature:
  - 
    value: 740
durability: 3
hardness:
  - 
    type: Vickers
    value: 4320000000

About Isuzu Glass Ltd.

Established in 1905 and headquartered in Osaka, Japan, Isuzu Glass Ltd. specializes in manufacturing molded glass lenses and optical filters. Their product range includes colored optical glasses and lenses utilized in projectors, lasers, medical devices, sensors, semiconductors, and energy equipment.

Links