Kato et al. 2016: n(e) 0.633–10.6 µm

Wavelength: µm
 (0.6328–10.591)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2=7.27453+\frac{0.20413}{λ^2-0.10074}+\frac{1098.54}{λ^2-719.62}$$

Conditions

optical_component: e

Notes

Room temperature. Extraordinary optical constants (e).

References

K. Kato, V. Petrov, N. Umemura. Phase-matching properties of yellow color HgGa2S4 for SHG and SFG in the 0.944-10.5910 μm range. Appl. Opt. 55, 3145-3148 (2016)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Mercury gallium sulfide

Mercury gallium sulfide (HgGa2S4) is a ternary compound notable for its non-linear optical properties. It is primarily used in optical applications, such as frequency conversion and phase matching in laser systems. The compound's non-linear optical coefficients make it suitable for second harmonic generation (SHG) and other non-linear processes. However, the presence of mercury in the compound necessitates careful handling due to toxicity risks. Research into this material often focuses on optimizing its non-linear characteristics and improving its thermal and mechanical stability for optical applications.

Other names and variations

  • HgGa2S4
  • Mercury thiogallate
  • Mercury gallium sulphide