Optical constants of HfO2 (Hafnium dioxide, Hafnia)
Al-Kuhaili 2004: n 0.2–2.0 µm

Wavelength: µm
 (0.2–2)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.875+6.28\text{×}10^{-3}λ^{-2}+5.80\text{×}10^{-4}λ^{-4}$$

Comments

Thin films of hafnium oxide deposited by electron beam evaporation.

References

M. F. Al-Kuhaili. Optical properties of hafnium oxide thin films and their application in energy-efficient windows. Opt. Mat. 27, 383-387 (2004)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Hafnium dioxide

Hafnium dioxide (HfO2) is a high-index, low-absorption material used extensively in optical applications. It is especially valuable for making thin-film dielectric coatings for mirrors, anti-reflective coatings, and beam splitters. Due to its excellent thermal stability and resistance to chemical corrosion, it is well-suited for harsh environments. Additionally, its high refractive index makes it an attractive material for planar waveguides and other integrated optics components. Beyond its optical uses, hafnium dioxide is also a key material in the fabrication of advanced gate dielectrics in field-effect transistors, contributing to the miniaturization and performance improvement of electronic devices.

Other names and variations:
  • HfO2
  • Hafnia
  • Hafnium(IV) oxide
  • Hafnium oxide