Optical constants of He (Helium)
Mansfield and Peck 1969: n 0.480–2.06 µm

Wavelength: µm
 (0.4801–2.0586)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n-1=\frac{0.01470091}{423.98-λ^{-2}}$$

Conditions

temperature: 273.15
pressure: 101325

Notes

Standard conditions: 0 °C, 760 torr (101.325 kPa).

References

C. R. Mansfield and E. R. Peck. Dispersion of helium. J. Opt. Soc. Am. 59, 199-203 (1969)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Helium

Helium (He) is a noble gas that is colorless, odorless, and tasteless. In the realm of optics, helium is frequently employed as a buffer gas in gas lasers such as helium-neon (He-Ne) and carbon dioxide (CO2) lasers. In He-Ne lasers, helium helps to excite neon atoms, thereby facilitating the laser action, while in CO2 lasers, it assists in the quick dissipation of heat. Additionally, helium's low refractive index, which is close to that of a vacuum, makes it useful in interferometry and other precision measurement techniques. Outside of optics, helium is commonly used in cryogenic environments to achieve extremely low temperatures, which are essential for certain high-precision devices like superconducting magnets used in Magnetic Resonance Imaging (MRI). Despite being one of the most abundant elements in the universe, its applications are quite diverse.