RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of HOYA - Optical glass
LAF2

Wavelength: µm
 (0.320–1.550)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=2.9657374-0.0096571624λ^{2}+0.026024525λ^{-2}+0.00036684641λ^{-4}+2.8205551\text{×}10^{-05}λ^{-6}-1.3739929\text{×}10^{-07}λ^{-8}$$

Conditions

temperature: 293

Notes

General glass Type

References

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

Properties of LAF2

thermal_dispersion:
  - 
    type: formula A
    coefficients: 2.21119e-06 0.0 0.0 0.0 0.0 0.0
nd: "1.74400"
Vd: "44.90"
glass_code: 744449
density:
  - 
    value: 4390
thermal_expansion:
  - 
    temperature_range: 243 343
    value: 7.2E-6
  - 
    temperature_range: 293 573
    value: 8.7E-6
dPgF: -0.0044
resistance:
  climatic: "1.0"
  stain: "2.0"
  acid: "3.0"

About

HOYA Corporation is a global technology company based in Japan, known for its diverse range of products in the fields of healthcare and optics. In the optical industry, HOYA is particularly recognized for its high-quality optical glass and lens technologies. The company produces a wide array of optical products, from eyeglass lenses with advanced coatings to specialized glass materials used in cameras, telescopes, and other precision optical instruments. HOYA's expertise extends to various types of optical glass, including low-dispersion and high-refractive-index materials, which find applications in situations requiring exceptional optical clarity and performance. Beyond its contributions to optics, HOYA has also ventured into medical technologies, making it a multi-faceted company with a broad impact. With a commitment to innovation and quality, HOYA has earned a reputation as a leader in its field, consistently delivering products that set industry standards for performance and reliability. Their expansive portfolio and technological prowess make them a go-to provider for both consumer and industrial optical solutions.

Links