RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of HIKARI - Optical glass
P-LASFH18S

Wavelength: µm
 (0.330–2.400)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=3.32566886-0.0131396072λ^{2}+0.0340298328λ^{-2}+0.000803745646λ^{-4}+1.03681091\text{×}10^{-05}λ^{-6}+2.05840857\text{×}10^{-06}λ^{-8}-0.000123587896λ^{4}$$

Conditions

temperature: 296

Notes

Low Tg glass

References

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

Properties of P-LASFH18S

nd: "1.851170"
Vd: 40.049954
glass_status: preferred
density:
  - 
    value: 5270
thermal_expansion:
  - 
    temperature_range: 243 343
    value: 7.3E-6
dPgF: -0.0072

About

Hikari Glass Co., Ltd. is a Japanese company specializing in the manufacturing of high-quality optical glass and optical components, and is a subsidiary of Nikon Corporation. Known for its precision engineering and strict quality control, Hikari serves various industries including consumer electronics, scientific research, and industrial optics. The company offers a wide range of specialized optical materials, including various types of crown and flint glasses, which are used in applications demanding high levels of optical clarity and performance. Hikari's products often find use in lenses, prisms, and other optical elements where precision and reliability are critical. With the backing of Nikon's renowned expertise in optics and imaging, Hikari has become a respected name in the field of optics, serving both domestic and international markets. Their expertise in crafting custom solutions for complex optical requirements has made them a preferred choice for organizations in need of specialized glass materials. As a testament to their commitment to quality, Hikari Glass Co., Ltd. is often sought after for projects requiring the highest levels of optical performance and integrity.

Links