Optical constants of Hydrogenated amorphous carbon
Smith 1984: Annealed at 450 °; n,k 0.261–0.827 µm
Wavelength:
µm
(0.261–0.827)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions
substrate: fused_quartz
Notes
Annealed (Ta = 450 °C)
References
F. W. Smith. Optical constants of a hydrogenated amorphous carbon film. J. Appl. Phys. 55, 764 (1984)