Optical constants of H2O:C3H5(OH)3 (Water:Glycerol)
Gupta et al. 2022: n 0.40–0.71 µm; 50 wt% glycerol

Wavelength: µm
 (0.4–0.71)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.38412+3.87705346\text{×}10^{-3}λ^{-2}-4.88915\text{×}10^{-5}λ^{-4}$$

Notes

50 wt% glycerol in water. Room temperature.

References

V. Gupta, O. Aftenieva, P. T. Probst, S. Sarkar, A. M. Steiner, N. Vogel, A. Fery, T. A. F. König. Advanced colloidal sensors enabled by an out-of-plane lattice resonance. Adv. Photonics Res. 2022, 2200152 (see supporting information)