Optical constants of H2O:C3H5(OH)3 (Water:Glycerol)
Gupta et al. 2022: n 0.40–0.71 µm; 0 wt% glycerol
Wavelength:
µm
(0.4–0.71)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n=1.32334+3.19237121\text{×}10^{-3}λ^{-2}-4.78767106898\text{×}10^{-6}λ^{-4}$$Notes
Water. Room temperature.
References
V. Gupta, O. Aftenieva, P. T. Probst, S. Sarkar, A. M. Steiner, N. Vogel, A. Fery, T. A. F. König. Advanced colloidal sensors enabled by an out-of-plane lattice resonance. Adv. Photonics Res. 2022, 2200152 (see supporting information)