RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of H2O, D2O (Water, heavy water, ice)
Wang et al. 2016: Heavy water; k 1.2–2.6 µm

Wavelength: µm
 (1.200–2.600)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

temperature: 295

Notes

22 °C.

References

Y. Wang, W. Wen, K. Wang, P. Zhai, P. Qiu, K. Wang. Measurement of absorption spectrum of deuterium oxide (D2O) and its application to signal enhancement in multiphoton microscopy at the 1700-nm window. Appl. Phys. Lett. 108, 021112 (2016)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information