Optical constants of H2O, D2O (Water, heavy water, ice)
Kedenburg et al. 2012: Heavy water; n 0.5–1.6 µm, k 0.5–1.75 µm

Wavelength: µm
 (0.5–1.75)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{-0.30637λ^2}{λ^2+47.26686}+\frac{0.74659λ^2}{λ^2-0.00893}$$

Conditions

temperature: 293

Comments

Heavy water (D2O) at 20 °C.

References

S. Kedenburg, M. Vieweg, T. Gissibl, H. Giessen. Linear refractive index and absorption measurements of nonlinear optical liquids in the visible and near-infrared spectral region. Opt. Mater. Express 2, 1588-1611 (2012)