Optical constants of H2O, D2O (Water, heavy water, ice)
Kedenburg et al. 2012: Water; n 0.5–1.6 µm, k 0.5–1.75 µm; 20.0 °C
Complex refractive index (n+ik)
Derived optical constants
Dispersion formula
$$n^2-1=\frac{0.75831λ^2}{λ^2-0.01007}+\frac{0.08495λ^2}{λ^2-8.91377}$$Conditions
temperature: 293
Notes
Distilled water at 20 °C.
References
S. Kedenburg, M. Vieweg, T. Gissibl, H. Giessen. Linear refractive index and absorption measurements of nonlinear optical liquids in the visible and near-infrared spectral region. Opt. Mater. Express 2, 1588-1611 (2012)
Data
Additional information
About Water
Water (H2O) is the most abundant compound on Earth's surface. It exists in various states—liquid, solid (ice), and gas (water vapor)—each having unique optical properties. In its liquid form, water is transparent over a broad range of visible wavelengths but absorbs infrared and ultraviolet light. It serves as the basis for many solvents used in optical spectroscopy. Ice, the solid state of water, also has specific optical characteristics like birefringence and is studied for its role in atmospheric optics. Water vapor, on the other hand, can act as a selective absorber of certain wavelengths and is significant in remote sensing applications. Given its ubiquity and importance in life sciences and environmental science, understanding the optical properties of water and its various states is crucial.
Other names and variations
- H2O
- Ice
Links