Optical constants of H2O, D2O (Water, heavy water, ice)
Afsar and Hasted 1977: Water; n,k 22.22–1733 µm; 19.0 °C

Wavelength: µm
 (22.22–1733)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

temperature: 292

Notes

Liquid water (H2O) at 19 °C

References

M. N. Afsar and J. B. Hasted. Measurements of the optical constants of liquid H2O and D2O between 6 and 450 cm−1. J. Opt. Soc. Am. 67, 902-904 (1977)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Water

Water (H2O) is the most abundant compound on Earth's surface. It exists in various states—liquid, solid (ice), and gas (water vapor)—each having unique optical properties. In its liquid form, water is transparent over a broad range of visible wavelengths but absorbs infrared and ultraviolet light. It serves as the basis for many solvents used in optical spectroscopy. Ice, the solid state of water, also has specific optical characteristics like birefringence and is studied for its role in atmospheric optics. Water vapor, on the other hand, can act as a selective absorber of certain wavelengths and is significant in remote sensing applications. Given its ubiquity and importance in life sciences and environmental science, understanding the optical properties of water and its various states is crucial.

Other names and variations

  • H2O
  • Ice

Links