Optical constants of H2O, D2O (Water, heavy water, ice)
Afsar and Hasted 1977: Heavy water; n,k 250–2000 µm
Wavelength:
µm
(250.0–2000)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions
temperature: 292.65
Notes
Heavy water (D2O) at 19.5 °C
References
M. N. Afsar and J. B. Hasted. Measurements of the optical constants of liquid H2O and D2O between 6 and 450 cm−1. J. Opt. Soc. Am. 67, 902-904 (1977)