RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of GeS2 (Germanium disulfide)
Slavich et al. 1989: n,k(a) 0.250–1.70 µm

Wavelength: µm
 (0.250–1.700)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

optical_component: a

Notes

Crystallographic a-axis. Experimental data.

References

A. S. Slavich, G. A. Ermolaev, I. A. Zavidovskiy, D. V. Grudinin, K. V. Kravtsov, M. K. Tatmyshevskiy, M. S. Mironov, A. N. Toksumakov, G. I. Tselikov, I. M. Fradkin, K. V. Voronin, M. R. Povolotskiy, O. G. Matveeva, A. V. Syuy, D. I. Yakubovsky, D. M. Tsymbarenko, I. Kruglov, D. A. Ghazaryan, S. M. Novikov, A. A. Vyshnevyy, A. V. Arsenin, V. S. Volkov, K. S. Novoselov. Germanium disulfide as an alternative high refractive index and transparent material for UV-visible nanophotonics. Light Sci. Appl., 14, 213 (2025) (See Supplementary Information)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Germanium disulfide

Germanium disulfide (GeS2) is a chalcogenide compound known for its wide infrared transparency and high refractive index. It crystallizes in an orthorhombic structure but is often used in its amorphous (glassy) form. GeS2-based glasses are key materials in infrared optics, especially in mid-IR applications (2–10 µm), due to their low phonon energy and favorable nonlinear optical properties. These characteristics make GeS₂ a valuable component in optical fibers, lenses, and infrared sensors. It is also studied for its role in photonics, infrared transmitting windows, and as a host material in rare-earth-doped fiber amplifiers.

Other names and variations

  • Germanium(IV) sulfide

Links