Optical constants of GaSb (Gallium antimonide)
Ferrini et al. 1998: n,k 0.207–2.48 µm
Wavelength:
µm
(0.207–2.480)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Notes
AlxGa1−xSb, x = 0 (GaAs). Thin film grown by molecular beam epitaxy on a GaSb substrate.
References
R. Ferrini, M. Patrini, S. Franchi. Optical functions from 0.02 to 6 eV of AlxGa1−xSb/GaSb epitaxial layers. J. Appl Phys. 84, 4517-4524 (1998)