Optical constants of GaS (Gallium sulfide)
Zotev et al. 2023: n,k(o) 0.36–1.0 µm
Complex refractive index (n+ik)
Derived optical constants
Conditions
optical_component: o
Notes
Multilayer crystals. In-plane (ordinary ray, o). Room temperature.
References
P. G. Zotev, Y. Wang, D. Andres-Penares, T. Severs-Millard, S. Randerson, X. Hu, L. Sortino, C. Louca, M. Brotons-Gisbert, T. Huq, S. Vezzoli, R. Sapienza, T. F. Krauss, B. D. Gerardot, A. I. Tartakovskii. Van der Waals materials for applications in nanophotonics. Laser and Photonics Rev. 17, 2200957 (2023) (Numerical data kindly provided by Panaiot Zotev)
Data
Additional information
About Gallium sulfide
Gallium sulfide (GaS) is a binary compound with a layered structure, belonging to the family of III-VI semiconductors. It has an indirect band gap of approximately 3.0 eV and is not as commonly used as other III-V compounds like GaAs or GaN. However, GaS exhibits intriguing optoelectronic and nonlinear optical properties, making it a material of interest for specialized applications. It can be synthesized in both crystalline and thin-film forms, and it has been explored for use in photodetectors and photovoltaic cells. While not a mainstream material, GaS is the subject of ongoing research aimed at uncovering its full potential for optoelectronic applications.
Other names and variations
- GaS
- Gallium (II) sulfide
Links