Optical constants of GaS (Gallium sulfide)
Kato and Umemura 2011: n(o) 0.633–10.6 µm
Complex refractive index (n+ik)
Derived optical constants
Dispersion formula
$$n^2=7.12996+\frac{0.26073}{λ^2-0.04627}+\frac{127.335}{λ^2-258.431}$$Conditions
optical_component: o
Notes
Room temperature. Ordinary optical constants (o).
References
K. Kato and N. Umemura. Sellmeier equations for GaS and GaSe and their applications to the nonlinear optics in GaSxSe1−x. Opt. Lett. 36, 746-747 (2011)
Data
Additional information
About Gallium sulfide
Gallium sulfide (GaS) is a binary compound with a layered structure, belonging to the family of III-VI semiconductors. It has an indirect band gap of approximately 3.0 eV and is not as commonly used as other III-V compounds like GaAs or GaN. However, GaS exhibits intriguing optoelectronic and nonlinear optical properties, making it a material of interest for specialized applications. It can be synthesized in both crystalline and thin-film forms, and it has been explored for use in photodetectors and photovoltaic cells. While not a mainstream material, GaS is the subject of ongoing research aimed at uncovering its full potential for optoelectronic applications.