Optical constants of GaP-InP (Gallium indium phosphide, GaInP)
Schubert et al. 1995: n,k 0.250–0.954 µm
Wavelength:
µm
(0.24961–0.95395)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Notes
Ga0.51In0.49P; Eg=1.85±0.2 eV; Room temperature.
References
M. Schubert, V. Gottschalch, C. M. Herzinger, H. Yao, P. G. Snyder, J. A. Woollam. Optical constants of GaxIn1−xP lattice matched to GaAs. J. Appl. Phys. 77, 3416 (1995)