RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of GaP-InP (Gallium indium phosphide, GaInP)
Kaneko and Kishino 1994: n 0.650–1.35 µm

Wavelength: µm
 (0.65–1.35)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{8.255228λ^2}{λ^2-0.315851^2}+\frac{0.151417λ^2}{λ^2-0.596868^2}$$

Conditions

substrate: GaAs

Comments

Averaged data for 580 nm and 851 nm GaInP films on a GaAs substrate.

References

Y. Kaneko and K. Kishino. Refractive indices measurement of (GaInP)m/(AlInP)m quasi‐quaternaries and GaInP/AlInP multiple quantum wells. J. Appl. Phys. 76, 1809-1818 (1994) (Digitization of graphical data and Sellmeier fit: Pedro Victor Sansoldo, University of Adelaide, Australia) [Calculation script (Python)]

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About