Optical constants of GaP (Gallium phosphide)
Parsons and Coleman 1971: n 54.4–366 µm

Wavelength: µm
 (54.369–366.03)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Room temperature

References

D. F. Parsons and P. D. Coleman. Far infrared optical constants of gallium phosphide. Appl. Opt. 10, 1683_1-1685 (1971)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Gallium phosphide, GaP

Gallium phosphide (GaP) is a binary III-V semiconductor with a direct bandgap of 2.26 eV, making it useful in specific optoelectronic applications. It is commonly employed in red, orange, and green light-emitting diodes (LEDs). One of the notable advantages of GaP is its high thermal conductivity, which allows for better heat dissipation in electronic devices. While it does not exhibit the same level of efficiency as materials like GaAs in high-frequency applications, GaP is used as a substrate material for other III-V semiconductors, such as GaAs and InP, to form heterostructure devices. It also finds applications in photonic integrated circuits and is sometimes used in combination with other semiconductors to engineer desired electronic or optical properties.

Other names and variations

  • Gallium(III) phosphide

Links