RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of Fe2O3 (Iron sesquioxide, Hematite)
Querry 1985: α-Fe2O3 (Hematite); n,k(o) 0.21–55.6 µm

Wavelength: µm
 (0.2100–90.9091)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

optical_component: o

Notes

α-Fe2O3 (Hematite). Ordinary optical constants (o).

References

M. R. Querry. Optical constants, Contractor Report CRDC-CR-85034 (1985)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Iron sesquioxide

Iron sesquioxide (Fe2O3), also known as ferric oxide or hematite, is a reddish-brown compound with various applications across industries. In optics, Fe2O3 is often used as a pigment in coatings and materials that require specific absorption or scattering properties. Its optically active properties have also made it a subject of study for photonic and plasmonic applications, particularly in the development of sensors and imaging technologies. Thin films of Fe2O3 have been investigated for use in optoelectronic devices and waveguides. While not a traditional optical material, iron sesquioxide provides specific characteristics beneficial to specialized optical applications and research.

Minerals: Hematite (haematite), Maghemite.

Other names and variations

  • Fe2O3
  • Iron(III) oxide
  • Diiron trioxide
  • Iron oxide
  • Ferric oxide
  • Ferric iron
  • Red iron oxide
  • Rouge
  • Colcothar
  • Rust
  • Ochre
  • Hematite
  • Haematite
  • Maghemite

Links