Optical constants of (C35H42N2S)n (F8BT)
Kamptner et al. 2024: n,k(e) 0.191–1.69 µm
Wavelength:
µm
(0.19146–1.68869)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions
optical_component: e
Notes
Extraordinary optical constants (e)
References
A. Kamptner, M. C. Scharber, M. Schiek. Accurate determination of the uniaxial complex refractive index and the optical band gap of polymer thin films to correlate their absorption strength and onset of absorption. Chem. Phys. Chem. e202400233 (2024) (Numerical data kindly provided by Manuela Schiek)
Data
Additional information
About (C35H42N2S)n
Other names and variations
- F8BT
- PFBT
- Poly(9,9-dioctyluorene-alt-benzothiadiazole)
- 2,1,3-benzothiadiazole-9,9-dioctylfluorene copolymer
- 9,9-dioctylfluorene-2,1,3-benzothiadiazole copolymer
- PFO-BT 15