Optical constants of EVASKY S87
Vogt et al. 2016: n,k 0.25–2.5 µm

Wavelength: µm
 (0.25–2.5)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Ethylene-vinyl acetate (EVA) with enhanced UV transmission. Room temperature.

References

  1. M. R. Vogt, H. Schulte-Huxel, D. Hinken, H. Holst, M. Winter, S. Blankemeyer, R. Witteck, M. Köntges, K. Bothe, R. Brendel. Optical constants of UV transparent EVA and the impact on the PV module output power under realistic illumination. Energy Procedia 92, 523-530 (2016)
  2. M. R. Vogt. Development of physical models for the simulation of optical properties of solar cell modules. PhD. Thesis (2015)