Optical constants of E7
Tkachenko et al. 2006: n(e) 0.532–1.7 µm
Wavelength:
µm
(0.532–1.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n=1.67798+0.01696λ^{-2}+0.00127λ^{-4}$$Conditions
optical_component: e
Notes
Extraordinary optical constants (e).
References
V. Tkachenko, G. Abbate, A. Marino, F. Vita, M. Giocondo, A. Mazzulla, F. Ciuchi, L. De Stefano. Nematic liquid crystal optical dispersion in the visible-near infrared range. Mol. Cryst. Liq. Cryst. 454, 263/[665]-271/[673], 2006