Optical constants of Dy2O3 (Dysprosium sesquioxide)
Medenbach et al. 2001: n 0.435–0.644 µm
Complex refractive index (n+ik)
Derived optical constants
Dispersion formula
$$n^2-1=\frac{2.7375λ^2}{λ^2-0.019984}$$References
O. Medenbach, D. Dettmar, R. D. Shannon, R. X. Fischer, W. M. Yen. Refractive index and optical dispersion of rare earth oxides using a small-prism technique. J. Opt. A: Pure Appl. Opt. 3, 174-177, 2001
Data
Additional information
About Dysprosium sesquioxide
Dysprosium sesquioxide (Dy2O3) is a rare-earth oxide that can exist in several crystalline phases. Its optical properties, such as a high refractive index and low absorption coefficients in the infrared region, make it interesting for specialized optical applications. It is also used as a raw material for producing dysprosium metal and various dysprosium compounds. Dy2O3 can be incorporated into glass, ceramics, and crystal hosts to modify their optical, electrical, and mechanical properties. While not as commonly encountered as other rare-earth oxides in optical applications, its unique characteristics make it a material of interest for future developments in both academia and industry.
Other names and variations
- Dy2O3
- Dysprosium(III) oxide
- Didysprosium trioxide
- Dysprosium oxide
Links