RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of D2O:C3H5(OH)3 (Heavy water:Glycerol)
Sarkar et al. 2022: n 0.40–0.71 µm; 50 wt% glycerol

Wavelength: µm
 (0.4–0.71)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n=1.38922+3.5200536\text{×}10^{-3}λ^{-2}-1.58701\text{×}10^{-5}λ^{-4}$$

Notes

25 wt% glycerol. Room temperature.

References

S. Sarkar, A. K. Ghosh, M. Adnan, O. Aftenieva, V. Gupta, A. Fery, J. Joseph, T. A. F. König. Enhanced figure of merit via hybridized guided-mode resonances in 2D-metallic photonic crystal slabs. Adv. Optical Mater. 2022, 2200954 (see supporting information)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information