Optical constants of D2O:C3H5(OH)3 (Heavy water:Glycerol)
Sarkar et al. 2022: n 0.40–0.71 µm; 25 wt% glycerol
Wavelength:
µm
(0.4–0.71)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n=1.35324+3.24537233\text{×}10^{-3}λ^{-2}-2.14761\text{×}10^{-5}λ^{-4}$$Notes
25 wt% glycerol. Room temperature.
References
S. Sarkar, A. K. Ghosh, M. Adnan, O. Aftenieva, V. Gupta, A. Fery, J. Joseph, T. A. F. König. Enhanced figure of merit via hybridized guided-mode resonances in 2D-metallic photonic crystal slabs. Adv. Optical Mater. 2022, 2200954 (see supporting information)