Boyd et al. 1971: n(o) 0.55–11.5 µm; 20 °C

Wavelength: µm
 (0.55–11.5)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=2.9064+\frac{2.3065λ^2}{λ^2-0.1149}+\frac{1.5479λ^2}{λ^2-738.43}$$

Conditions

temperature: 293
optical_component: o

Notes

Ordinary optical constants (o); 20 °C

References

  1. G. D. Boyd, H. Kasper, J. H McFee. Linear and nonlinear optical properties of AgGaS2, CuGaS2, and CuInS2, and theory of the wedge technique for the measurement of nonlinear coefficients. IEEE J. Quantum Electron., 7, 563-573 (1971)
  2. G. C. Bhar and G. Ghosh. Temperature-dependent Sellmeier coefficients and coherence lengths for some chalcopyrite crystals. J. Opt. Soc. Am. 69, 730-733 (1979)
  • Ref. 2 provides a dispersion formula based on data from Ref. 1

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Copper gallium sulfide

Copper gallium sulfide (CuGaS2) is a ternary compound semiconductor that exhibits a chalcopyrite crystal structure. This material is notable for its non-linear optical properties and is frequently employed in non-linear frequency conversion applications such as second-harmonic generation and parametric down-conversion. Its large non-linear coefficients and extensive phase-matching capabilities make it an ideal choice for infrared and mid-infrared applications. The material also boasts high thermal conductivity and damage threshold, which lends itself well to high-power optical systems. While not as commonly used as some other non-linear optical materials, copper gallium sulfide remains a specialized choice for applications requiring efficient non-linear frequency conversion, particularly in the infrared spectrum.