Optical constants of CuGaS2 (Copper gallium sulfide)
Boyd et al. 1971: n(e) 0.55–11.5 µm; 120 °C
Complex refractive index (n+ik)
Derived optical constants
Dispersion formula
$$n^2-1=3.4834+\frac{1.7316λ^2}{λ^2-0.1453}+\frac{1.7785λ^2}{λ^2-738.43}$$Notes
Extrardinary optical constants (e); 120 °C
References
- G. D. Boyd, H. Kasper, J. H McFee.
Linear and nonlinear optical properties of AgGaS2, CuGaS2, and CuInS2, and theory of the wedge technique for the measurement of nonlinear coefficients.
IEEE J. Quantum Electron., 7, 563-573 (1971)
- G. C. Bhar and G. Ghosh. Temperature-dependent Sellmeier coefficients and coherence lengths for some chalcopyrite crystals.
J. Opt. Soc. Am. 69, 730-733 (1979)
- Ref. 2 provides a dispersion formula based on data from Ref. 1
Data
Additional information
About Copper gallium sulfide
Copper gallium sulfide (CuGaS2) is a ternary compound semiconductor that exhibits a chalcopyrite crystal structure. This material is notable for its non-linear optical properties and is frequently employed in non-linear frequency conversion applications such as second-harmonic generation and parametric down-conversion. Its large non-linear coefficients and extensive phase-matching capabilities make it an ideal choice for infrared and mid-infrared applications. The material also boasts high thermal conductivity and damage threshold, which lends itself well to high-power optical systems. While not as commonly used as some other non-linear optical materials, copper gallium sulfide remains a specialized choice for applications requiring efficient non-linear frequency conversion, particularly in the infrared spectrum.
Other names and variations
- CuGaS2
- Copper gallium disulfide