Optical constants of Cu-Zn (Copper-zinc alloy, Brass)
Querry 1985: n,k 0.21–55.6 µm; 70% Cu 30% Zn
Complex refractive index (n+ik)
Derived optical constants
Notes
70% Cu, 30% Zn.
References
M. R. Querry. Optical constants, Contractor Report CRDC-CR-85034 (1985)
Data
Additional information
About Copper-zinc alloy
Brass is an alloy primarily composed of copper and zinc, prized for its versatility and attractive gold-like appearance. Its mechanical properties, such as strength and ductility, can be adjusted by varying the copper-to-zinc ratio, making it suitable for a wide range of applications—from musical instruments and decorative pieces to plumbing and marine hardware. Brass is relatively resistant to corrosion and easy to machine, further contributing to its popularity in manufacturing and engineering fields. In decorative contexts, the natural patina that can develop on brass adds to its aesthetic appeal and cultural significance.