Optical constants of Cu:C12H4N4 (Copper:tetracyanoquinodimethane, Cu:TCNQ )
Querry 1985: n,k 0.21–55.6 µm
Wavelength:
µm
(0.2100–55.5556)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Notes
Copper:Tetracyanoquinodimethane (Cu:TCNQ).
References
M. R. Querry. Optical constants, Contractor Report CRDC-CR-85034 (1985)
Data
Additional information
About Copper:tetracyanoquinodimethane
Other names and variations
- Cu:TCNQ
- Cu:C12H4N4
Links