Optical constants of Cu (Copper)
Hagemann et al. 1974: n,k 0.0000248–248 µm
Complex refractive index (n+ik)
Derived optical constants
References
- H.-J. Hagemann, W. Gudat, C. Kunz.
Optical constants from the far infrared to the x-ray region: Mg, Al, Cu, Ag, Au, Bi, C, and Al2O3.
J. Opt. Soc. Am. 65, 742-744 (1975)
- H.-J. Hagemann, W. Gudat, C. Kunz. [DESY report SR-74/7 (1974)](https://refractiveindex.info/download/data/1974/Hagemann 1974 - DESY report SR-74-7.pdf)
Data
Additional information
About Copper
Copper (Cu) is a highly versatile transition metal with excellent electrical and thermal conductivity. While its primary applications span electrical wiring, plumbing, and various industrial machinery, it also finds specialized uses in optics. Notably, polished, bare copper is often the material of choice for high-power infrared mirrors, including those used in CO2 lasers, due to its high reflectivity in the infrared spectrum and exceptional thermal resilience. The metal's malleability and corrosion resistance further allow it to be shaped into intricate forms, making it invaluable across a range of industries. Whether in general construction or specific niches like high-power optical components, copper's multifaceted properties make it a material of critical importance.
Other names and variations
- Cu
Links