RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of CsPbCl3 (Cesium lead trichloride)
Zhang et al. 2023: n,k 0.193–1.69 µm

Wavelength: µm
 (0.1930–1.6900)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

film_thickness: 1.98E-7
substrate: glass

Notes

Vapor-deposited thin film. Film thickness: 198 nm; Room temperature

References

X. Zhang, Y. Chen, X. Liu, Z. Liu, H. Gu, S. Bo, G. Liao. Optimizing the design of the vapor-deposited CsPbCl3-based optoelectronic devices via simulations and experiments. Adv. Funct. Mater., 2310945 (2023) (Numerical data kindly provided by Xuning Zhang)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Cesium lead trichloride

About Perovskite