Optical constants of CsPbCl3 (Cesium lead trichloride)
Ermolaev et al. 2023: n,k(o) 0.400–0.800 µm
Wavelength:
µm
(0.400–0.800)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions
optical_component: o
Notes
CsPbCl3 monocrystal. Ordinary optical constants (o).
References
G. Ermolaev, A. P. Pushkarev, A. Zhizhchenko, A. A. Kuchmizhak, I. Iorsh, I. Kruglov, A. Mazitov, A. Ishteev, K. Konstantinova, D. Saranin, A. Slavich, D. Stosic, E. S. Zhukova, G. Tselikov, A. D. Carlo, A. Arsenin, K. S. Novoselov, S. V. Makarov, V. S. Volkov. Giant and tunable excitonic optical anisotropy in single-crystal halide perovskites. Nano Lett. 23, 2570–2577 (2023) (Numerical data kindly provided by Georgy Ermolaev)