Optical constants of CsPbBr3 (Cesium lead tribromide)
Brennan et al. 2024: n,k 0.200–2.50 µm
Wavelength:
µm
(0.200–2.500)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Notes
Likely crystal orientation: <251>; Bridgman-grown, polished crystal; Room temperature.
References
M. C. Brennan, D. M. Krein, E. Rowe, C. L. McCleese, L. Sun, K. G. Berry, P. R. Stevenson, M. A. Susner, T. A. Grusenmeyer. Fundamental optical constants and anti-reflection coating of melt-grown, polished CsPbBr3. MRS Commun. ASAP (2024) (See Supplementary Information)
Data
Additional information
About Cesium lead tribromide
Other names and variations
- CsPbBr3
Links