Optical constants of Cs (Caesium)
Monin and Boutry 1974: n,k 0.254–0.620 µm; 195 K

Wavelength: µm
 (0.2536–0.6200)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

temperature: 195

Notes

195 K (-78.15 °C)

References

J. Monin and G.-A. Boutry. Optical and photoelectric properties of alkali metals. Phys. Rev. B 9, 1309-1327 (1974)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Caesium

Caesium (Cs) is an alkali metal characterised by its softness and extremely low melting point for a metal, just above room temperature at 28.5 °C (83.3 °F). It is silvery-gold in colour and highly reactive, especially with water, leading to its storage in mineral oil or inert gases. In the realm of technology, caesium is crucial for the operation of atomic clocks, which use the microwave spectral line emitted by electrons in caesium atoms to define the second, the base unit of time. Due to the high precision of caesium-based atomic clocks, they serve as the timekeeping standard for global navigation satellite systems like GPS. Caesium is also used in photoelectric cells, ion propulsion systems, and as a catalyst in certain organic reactions. Despite its technological utility, caesium compounds must be handled with care as they can be corrosive and pose health risks upon exposure. Overall, caesium is a fascinating element whose unique properties make it indispensable in precision timekeeping and various specialised applications.