RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of CdTe (Cadmium telluride)
DeBell et al. 1979: n 6–22 µm; 20 K

Wavelength: µm
 (6–22)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{6.0599879λ^2}{λ^2-0.1004272}+\frac{3.7564378λ^2}{λ^2-6138.789}$$

Notes

20 K (-253.1 °C)

References

A. G. DeBell, E. L. Dereniak, J. Harvey, J. Nissley, J. Palmer, A. Selvarajan, W. L. Wolfe. Cryogenic refractive indices and temperature coefficients of cadmium telluride from 6 µm to 22 µm. Appl. Opt. 18, 3114-3115 (1979)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Cadmium telluride

Cadmium telluride (CdTe) is an inorganic compound that typically crystallizes in a cubic zincblende structure. It is a direct bandgap semiconductor with a bandgap energy of approximately 1.5 eV, making it highly suitable for photovoltaic applications, especially thin-film solar cells. CdTe solar cells are commercially significant due to their lower manufacturing costs and competitive efficiency levels compared to silicon-based cells. Besides photovoltaics, CdTe is also employed in infrared detectors, radiation detectors, and electro-optic modulators. However, the presence of cadmium, a toxic heavy metal, calls for stringent handling and disposal protocols and has prompted research into recycling methods. Synthesis methods for CdTe include physical vapor deposition, chemical vapor deposition, and close-spaced sublimation, among others, each offering unique advantages in terms of film quality and manufacturing scalability. Despite the environmental concerns related to its toxicity, CdTe remains a highly relevant material in renewable energy technologies and continues to attract research efforts aimed at mitigating its environmental impact.

Other names and variations

  • CdTe

Links