RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of CdSe/ZnCdS (Cadmium selenide / zinc cadmium sulfide core/shell)
Aftenieva et al. 2023: n,k 0.350–1.20 µm

Wavelength: µm
 (0.3500–1.2000)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Cadmium selenide and zinc cadmium sulfide (CdSe/ZnCdS) core/shell quantum dots

References

O. Aftenieva, M. Sudzius, A. Prudnikau, M. Adnan, S. Sarkar, V. Lesnyak, K. Leo, A. Fery, T. A. F. König. Lasing by template-assisted self-assembled quantum dots. Adv. Opt. Mater. 2202226 (2023) (Numerical data kindly provided by Tobias König)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Cadmium selenide / zinc cadmium sulfide core/shell quantum dots

Other names and variations

  • CdSe/ZnCdS

Links